galvanic corrosion

Status
Not open for further replies.
Jan 22, 2008
21
Macgregor 26X PORT DICKSON - MALAYSIA MA
Hi All,

I have a 2008 Hunter 33 and have replaced 4 pcs anode since new. Is there something wrong with my electrical system or it is just a common issue among boaters. Someone suggest to hang an anode to the side of the boat and ground it to negative. Your advice on this matter is much appreciated. Sonny:confused:
 

natotm

.
May 5, 2006
29
- - -
If you're in a marina and there is stray current coming from other boats in your vicinity that's the price to pay. If you are not around other boats that level of zinc loss seems high. There is a test to find excess voltage around your boat and a marina may have it.

My experience with this is that if I am in a marina for awhile I make sure to check/change the zincs often. At Daytona Beach I went through 2 zincs in a quarter. Now, in the Caribbean, I do 2 zincs a year.

Your boat should be protected from itself but you may need to check your system if there are no other "leakers" near you.

Good luck
 
Sep 25, 2008
7,752
Alden 50 Sarasota, Florida
Sonny
Before jumping to conclusions regarding why, do an archive search here for "galvanic". There is far too much info there to repeat but worth reading and will give you a better idea what to look for and how to fix it be it your boat or some outside source
 
Jan 22, 2008
21
Macgregor 26X PORT DICKSON - MALAYSIA MA
Hi All,
Yes, my boat is park in the marina. I use the shore power once a week to top up my batteries and sometime use the air cond. My neighbour, a Beneteau 343, same year model as mine and yet to replace his anode. Will check out the "Galvanic" in the forum. Thanks.
 

RJ9757

.
Jun 15, 2004
29
- - San Francisco
electrolysis issues

I've recently experienced a similar problem on my boat, which has been in the same slip for the last several years but has recently started consuming zincs at an alarming and unprecedented rate. Here's a couple of things that I've learned:

You can use a Corrosion Reference Electrode (available fairly cheaply from various outlets, including boatzincs.com) to determine if your boat is adequately protected, and if not, where the problem originates, e.g. stray electrical currents from neighboring boats.

In the meantime, you can get a zinc 'Grouper' for about $40 at West Marine that you can hang over the side for additional protection.

Good luck! Keep us posted!
 
Status
Not open for further replies.