T
Tony Helbling
We bought our H30 this past summer... during the survey haul-out, we replaced the zincs on the drive shaft and noted some small rust spots on the wing keel. (The boat was in saltwater for 10 years prior to purchase.) We put it back in for only two months before moving it to the freshwater Columbia River. We trucked it down I-5 and just before putting her back in, we noticed that those two month old zincs looked like 2 year old zincs. The spots on the keel had multiplied 2 or 3 times... I checked both the AC and DC electrical systems to ensure there was no path to ground... it was good. I am suspecting the VHF as this is the only way for any energy to get to the keel (through the mast). Possibly it could have been someone elses problem in the next slip, but I am open for suggestions...!!!!????