I just got "done" priming my hull. I bought this primer because it was touted as being ideal for water based ablative. I will go on record as saying this product is the worst paint product I have EVER used, bar none. Ten minutes of power stirring and it comes out as thick as cake batter and as clumpy as can be. Dries almost instantly when exposed to air so the clumps start pealing off the roller too. Then it doesn't cover worth beans. I'll have to sand the entire hull again just to get the clumps off. This was supposed to be, prime, wait two hours, paint. Not any more!
If others have had better results, please post to counter my bad press, but I just HAD to tell my story.