I had my bottom sanded and painted back in Dec 2012 and back in water Jan 2013 with sea hawk BIOCOP and so was suppose to have diver clean in 90 days
but was delayed until today and so the diver said looked great and just some minor slime.
I will have it cleaned every 6 or 8 weeks,the diver did clean my bottom back in sept and back than the hull looked except for all the barnacles all over the hull.
2 years befor I had used Pettit SR60 and was not very happy with it's performance and had many barnacles on the water line and hull and dragged it out to try to last 2 years before a new bottom job.
I did not go with Trinadad SR because it is a hard bottom paint and worried about it building up over the years,many PGSC member do use Trinadad SR and are very happy with it and tell me they just give it a real good sanding when needing a new bottom job,the other reason is that pettit tells you you need to remove all Antfouling paint before putting on SR hard bottom paint and I called them and they said to just give a real good sanding before painting over a antifouling paint with SR hard.
I choose BIOCOP because of others claiming how good it worked here in PG.
Nick
but was delayed until today and so the diver said looked great and just some minor slime.
I will have it cleaned every 6 or 8 weeks,the diver did clean my bottom back in sept and back than the hull looked except for all the barnacles all over the hull.
2 years befor I had used Pettit SR60 and was not very happy with it's performance and had many barnacles on the water line and hull and dragged it out to try to last 2 years before a new bottom job.
I did not go with Trinadad SR because it is a hard bottom paint and worried about it building up over the years,many PGSC member do use Trinadad SR and are very happy with it and tell me they just give it a real good sanding when needing a new bottom job,the other reason is that pettit tells you you need to remove all Antfouling paint before putting on SR hard bottom paint and I called them and they said to just give a real good sanding before painting over a antifouling paint with SR hard.
I choose BIOCOP because of others claiming how good it worked here in PG.
Nick