I'm about to gelcoat a repaired mast step. I have a little bit of experience with it and understand the overall process but I do have a few questions...
Setup
Questions
Setup
- Gelcoat with wax
- Tint kit
- 404 & 406 filler
- Styrene
- Two Preval Sprayers
Questions
- When thickening, how much does the thickener affect the color? Can 404 or 406 be used as a thickener? I've seen many sites say that the gouge, scratch, etc should be filled and sanded flat before applying gelcoat. This means that the filler and resin is level with the boat's existing gelcoat. Shouldn't there some room be left for gelcoat? This way you would sand the new gel even with the existing instead of sanding through it to make it level
- Does it need to be thickened for a vertical scratch or small gouge or can this be sprayed?
- When spraying, is there a limit to thickness? Will it kick faster if it's laid on thick?
- I assume sunlight affects heat and in turn, cure time?
- What's the expected time to cure in 85F?
- Can I recoat if the gelcoat before it fully cures if the gelcoat has wax in it?
- Any additional tips for applying gelcoat that you've learned from experience?